Skip to content

Redispersible Polymer Powder RDP Powder VAE Powder

If you are looking for high-quality products, please feel free to contact us and send an inquiry, email: brad@ihpa.net



Look: White powder N.W. : 25 kg/bag Use of redispersible plastic powder Improve flow properties Increased flexural strength Water absorption by material is reduced Concrete accelerator product introduction Dispersible plastic powder (RDP, VAE)is an white powdery material that’s commonly used in the modification and repair of mortars made from cement- or gypsum. Acetate ethylene redispersible dust may be rapidly redispersed to create an emulsion. After the addition of water, it will have the same properties. This is because the water evaporates as cement mortar coagulation and hardening, so the polymer particles stay in cement mortar. This film can act as a modified cement mortar emulsion. The film can be used to modify cement mortars and is weather-resistant, abrasion resistant, flexible, and adhesive.

Reusable polymer powders for

Can improve the construction performance of

Reversible polymer powdercan enhance flow performance; increase temperature and resist sags;

Reversible polymer powder may improve water retention and cohesion.

The effects of VAE Redispersible plastic powdercan after being cured

To increase the tensile, bend and strength of materials; to reduce their elastic modulus; to improve deformability; material compactness; material wear resistance; material cohesive strength; carbonization depth; material water absorption reduction; material with exceptional water-increasing capabilities (adding water increasing rubber dust).

Parameters redispersible plastic powder VAE powder Parameters Appearance White powder ≥98.0 Ash(wt%) 10±2% Bulk density(g/L) 300-500 325 6-8 Lowest temperature for film formation 0~5 Packaging and storage Redispersible plastic powder Redispersible Polymer Powder should be stored at room temperature. Redispersible polymer powder should be used for at least six months.

Please do not use when it is summer.

A hot, humid environment may increase the likelihood of agglomeration.

Please make sure to follow these instructions: Recommend As soon as the bag is opened, you should use r Empersible powder .

Bag with a 25kg/bag paper-plastic compound bottom valve.

Packaging could be tailored to customers’ requirements.


Inquiry us